The surface glossiness of FRP products is not good, and the common ones are: local dull patches appear, or the entire surface loses luster. The main reasons are: FRP products are released from the mold prematurely: or the release agent is not well selected; or the surface of the mold is not dry.
Production Method:
1. Before the mold is used, it should be fully polished. After waxing or polishing, the surface of the mold should be wiped off with a clean gauze;
2. After the product is fully cured, the demoulding begins;
3. The surface of the mold should be kept dry;